Outokumpu Moda 410S/4000 is a 13% Cr, ferritic stainless steel that is used in applications requiring good resistance to mildly corrosive environments. It is a low carbon, non-hardening modification of Type 410 stainless steel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on low and high temperature performance, corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1329. Producer or source: Outokumpu Oyj.