Abstract

Hitachi Metals SLD-Magic is a high-performance alloy cold-work tool steel that is characterized by improved mold lifespan and easy mold fabrication. This datasheet provides information on composition, physical properties, hardness, elasticity as well as fatigue. It also includes information on low and high temperature performance as well as heat treating, machining, and joining. Filing Code: TS-802. Producer or source: Hitachi Metals Ltd.