Abstract

Sandvik 12R10L is fully austenitic with a very low cobalt content for nuclear applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear and bend strength as well as fatigue. It also includes information on high temperature performance as well as heat treating. Filing Code: SS-1309. Producer or source: Sandvik Steel Company and Sandvik AB.