Olin Brass C76200 is a copper-nickel-zinc alloy developed to conserve nickel for national defense. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming. Filing Code: Cu-896. Producer or source: Olin Brass and Somers Thin Strip.