Abstract

Kaiser Alloy 6063 in pipe and tube is used in air cylinder lines. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as machining and joining. Filing Code: Al-458. Producer or source: Kaiser Aluminum Corporation. See also Alloy Digest Al-436, March 2011.