Nicrofer 6022 hMo, a Ni-Cr-Mo-Nb material also called Alloy 625H, is an alloy that combines high-creep strength with excellent corrosion-oxidation resistance. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Ni-753. Producer or source: VDM Metals International GmbH.