MANAURITE 900X is a casting alloy with good creep strength and high thermal shock resistance. This alloy is evolution from Manaurite 900 (Alloy Digest SS-1304, March 2019). This datasheet provides information on composition and physical properties as well as creep. It also includes information on high temperature performance as well as joining. Filing Code: SS-1305. Producer or source: Manoir Industries, Manoir Pîtres.