Abstract
YSS YXR7 is a high-speed tool steel with good toughness and wear resistance. It is used for blanking dies, forging dies, heading dies, and thread forming dies. This datasheet provides information on composition, physical properties, hardness, and bend strength. It also includes information on heat treating. Filing Code: TS-783. Producer or source: Hitachi Metals America, Ltd.