Abstract

Concast C95500 is a cast nickel-aluminum bronze alloy. Aluminum bronze is the highest strength standard copper-based alloy. The nickel content in C95500 greatly enhances its mechanical strength, and wear and corrosion resistance, making it suitable for heavyduty applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as machining and joining. Filing Code: Cu-900. Producer or source: Concast Metal Products Co..