Böhler (or Boehler) S700 tungsten-molybdenum high-speed tool steel has good wear resistance and red hardness. This datasheet provides information on composition and physical properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-778. Producer or source: Voestalpine BÖHLER Edelstahl GmbH & Co KG.