Abstract

Sandvik Sanicro 25 is an austenitic stainless steel with excellent high-temperature properties and was designed for use in superheaters and reheaters in high-efficiency-coal fired plants. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance. Filing Code: SS-1293. Producer or source: Sandvik Steel Company and Sandvik AB.