Strenx 900 is a structural steel that guarantees a minimum yield strength of up to 900 MPa (131 ksi) depending on thickness. Strenx 900 provides a good combination of strength and toughness together with excellent workshop properties. Typical applications include load-bearing structures, where low weight is needed. It meets the requirements of EN 10 025-6 for the S890 grade and thicknesses. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-821. Producer or source: SSAB Swedish Steel Inc. and SSAB Tunnplat AB.