Abstract

Wieland K60 is an age hardenable copper alloy combining good electrical and thermal conductivity with high strength. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well as heat treating and machining. Filing Code: Cu-878. Producer or source: Wieland Metals Inc..