Abstract

Strenx 700 MC PLUS is a hot-rolled structural steel made for cold forming, with minimum yield strength of 700 MPa (102 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S700MC in EN 10149-2. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on surface qualities. Filing Code: SA-817. Producer or source: SSAB Swedish Steel Inc..