Abstract

Magnesium K1A is the casting alloy with the highest vibration-damping index. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as casting, machining, and joining. Filing Code: Mg-85. Producer or source: Multiple producers.