Manaurite 36X is cast stainless steel with a composition (26Cr-35Ni) that makes it resistant to both oxidizing and carburizing atmospheres at high temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: SS-1286. Producer or source: Manoir Pîtres.