Abstract

AZ91E is a general-purpose sand and investment casting alloy. This datasheet provides information on composition, physical properties, and bend strength. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-83. Producer or source: Multiple producers.