Abstract

YSS DAC 55 is a standard grade for die casting dies. Tool steel for large or squeeze die casting molds with excellent heat crack resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on heat treating. Filing Code: TS-747. Producer or source: Hitachi Metals America Ltd.