Abstract

Alloy CuSn6Zn6 is bronze alloy for the electrical industry. Typical uses include electrical devices, switching elements, contact springs, relay springs, leaf springs, and switching elements. This datasheet provides information on composition and physical properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Cu-882. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.