Ferrium C64 is a case-hardened gear steel with ultrahigh strength. It has surface wear properties and fatigue properties superior to those found in current commercial alloys. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance. Filing Code: SA-827. Producer or source: QuesTek Innovations, LLC.