Abstract

YSS DAC 40 high-strength aluminum extrusion die steel has higher strength and better softening resistance at elevated temperature than DAC. This datasheet provides information on composition and elasticity. It also includes information on heat treating. Filing Code: TS-746. Producer or source: Hitachi Metals America Ltd.