Abstract

TBL is a wear-resistant special structural steel with boron as heavy plate that is normalized with thicknesses up to 100 mm (3.9 in.) made of fine-grained structural steel TBL. This datasheet provides information on composition and tensile properties. It also includes information on forming and heat treating. Filing Code: SA-808. Producer or source: ThyssenKrupp Steel Europe AG.