NSSMC 845 is a 46Ni-23Cr-4W-Fe alloy with 3Cu for added corrosion resistance in reducing media. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: Ni-733. Producer or source: Sumitomo Metal USA Corporation.