Abstract

Alloy KHP 151 (UNS C15100) is a high performance copper alloy with very high conductivity. Typical uses include lead frames for high-power electronic circuits, connectors, and switchblade jaws; and applications requiring high conductivity, moderate strength, good bend formability and good stress relaxation resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-863. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.