Abstract
Sandvik Sanicro 32Cu is a corrosion resistant grade (CRA) available as billets. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1263. Producer or source: Sandvik Steel Company.