Abstract
Nimonic PE11 is a nickel-iron-chromium alloy that is precipitation hardened. It is used at high temperatures. This datasheet provides information on composition and physical properties. It also includes information on high temperature performance as well as forming. Filing Code: Ni-728. Producer or source: Special Metals Corporation.
This content is only available as a PDF.
Copyright © ASM International® 2017
2017
ASM International
You do not currently have access to this content.