Abstract

Thermodur E40K is a high quality special steel with excellent mechanical properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-744. Producer or source: Deutsche Edelstahlwerke GmbH.