Abstract

Alloy C688 is a high-performance copper alloy with very high conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Cu-867. Producer or source: Gebr. Kemper GmbH + Company KG Metallwerke.