YSS DAC3 is a standard grade for general use with good balance of toughness, strength at elevated temperature, and with excellent hardenability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as heat treating. Filing Code: TS-743. Producer or source: Hitachi Metals America Ltd.