Abstract

Sumitomo SMC276-125 (minimum yield strength of 125 ksi, or 862 MPa) is a high-strength nickel alloy (nominal 16% Mo) for use in oil country tubular goods as a material suitable for severe sour service. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: Ni-738. Producer or source: Nippon Steel and Sumitomo Metal Corporation.