Abstract

Kaiser alloy 5052 in pipe and tube is used in hydraulic lines. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, machining, and joining. Filing Code: Al-451. Producer or source: Kaiser Aluminum Corporation.