Abstract
Mueller Alloy C10100 is an oxygen-free copper used for automotive rectifiers and for electrical applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-851. Producer or source: Mueller Brass Company.
automotive rectifiers, bend strength, chemical composition, corrosion-resistant alloys, elasticity, electrical applications, hardness, heat treatability, joinability, machinability, MUELLER ALLOY C10100, oxygen free copper, physical properties, tensile properties, workability, thermal properties, UNS C10100