Abstract

Strenx 700MC is a hot-rolled structural steel made for cold forming, with minimum yield strength of 700 MPa (102 ksi) for stronger and lighter structures. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-763. Producer or source: SSAB Swedish Steel Inc..