Abstract

Vallourec VM 95 13Cr SS (minimum yield strength 95 ksi, or 655 MPa) is a super martensitic steel for use in oil country tubular goods as a material suitable for sour service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: CS-200. Producer or source: Vallourec USA Corporation.