Abstract
ATI 436S ferritic stainless is a single phase alloy in the same family as Type 409 and is common to many of those properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: SS-1244. Producer or source: Allegheny Ludlum.