Abstract

AK Steel Chromeshield 22 stainless steel combines the exceptional corrosion performance of a high chromium ferritic alloy with the enhanced ductility of AK Steel’s Ultra Form technology. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: SS-1242. Producer or source: AK Steel.