Abstract

Böhler (or Boehler) S600 high-speed steel is similar to M2 and has excellent toughness and cutting properties. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-737. Producer or source: Böhler Edelstahl GmbH & Company KG.