Abstract
Kobelco Alloy SuperKFC has high strength and high conductivity for electronic applications. The alloy is nominally Cu-0.3Fe-0.1P. This datasheet provides information on composition, physical properties, hardness, and tensile properties. and bend strength. It also includes information on forming. Filing Code: Cu-854. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business.