VDM NeutroShield is an austenitic stainless steel that is alloyed with boron to absorb neutrons. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-1255. Producer or source: VDM Metals GmbH.