UNSSMC NAR-305B is a nonmagnetic heat and corrosion-resistant austenitic stainless steel with high silicon. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1226. Producer or source: Nippon Steel and Sumitomo Metal Corporation.