Outokumpu Supra 316LN/4429 is a grade that can be used in applications with increased demand for corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1224. Producer or source: Outokumpu Stainless Bar Inc..