Pyromet alloy 706 has similarities to alloy 718, but improves fabricability and welding. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-723. Producer or source: Carpenter Specialty Alloys.