NSSMC is a high temperature alloy with noted resistance to metal dusting. This datasheet provides information on composition. It also includes information on corrosion resistance as well as forming and joining. Filing Code: SS-1216. Producer or source: Nippon Steel and Sumitomo Metal Corporation.