Amagnit 501 is a low carbon austenitic stainless steel designed to be nonmagnetic for many oil field components and accessories. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming. Filing Code: SS-1214. Producer or source: ThyssenKrupp Metallurgical Products USA.