Abstract
The specification DIPLUS-S stipulates the requirements for non-alloy structural steels above and beyond the minimum requirements stated in the EN 10025, Part 2 standard. The specification applies to the following grades in conformity to EN 10025, Part 2, in the thickness range stated: S235J0/J2, S275J0/J2, and S355J0/J2/K2 in thicknesses 6-250 mm (0.24-9.8 in.). This datasheet provides information on composition and physical properties as well as fracture toughness. It also includes information on heat treating. Filing Code: CS-189. Producer or source: Dillinger Hütte GTS.