Böhler (or Boehler) M461 Extra is a precipitation hardening steel grade for plastic molds with good machinability in the precipitation hardened condition. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on machining. Filing Code: TS-730. Producer or source: Böhler Edelstahl GmbH & Company KG.