Abstract

Wieland-UB7 is an aluminum bronze alloy with high hardness and compressive strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-836. Producer or source: Wieland Metals Inc..