XAR HT is a wear-resistant special structural steel as heavy plate that is quenched or quenched and tempered. It has good toughness and resistance to impact wear. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-723. Producer or source: ThyssenKrupp Steel Europe AG.