Abstract

Wieland-UB5 is an aluminum bronze alloy with good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Cu-835. Producer or source: Wieland Metals Inc..