Boehler M333 Isoplast is a plastic mold steel with low levels of impurities to meet high gloss surfaces at low costs. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating, machining, and joining. Filing Code: TS-729. Producer or source: Böhler Edelstahl GmbH & Company KG.